Journal of Dentistry
Volume 38, Issue 1 , Pages 16-22 , January 2010

A preliminary evaluation of the structural integrity and fracture mode of minimally prepared resin bonded CAD/CAM crowns

  • Effrosyni A. Tsitrou

      Affiliations

    • Department of Adult Dental Care, School of Clinical Dentistry, University of Sheffield, Claremont Crescent, S10 2TA, Sheffield, UK
    • Corresponding Author InformationCorresponding author. Tel.: +44 0114 271 7962; fax: +44 0114 266 5326.
  • ,
  • Maria Helvatjoglu-Antoniades

      Affiliations

    • Department of Operative Dentistry, School of Dentistry, Aristotle University of Thessaloniki, Thessaloniki, Greece
  • ,
  • Richard van Noort

      Affiliations

    • Department of Adult Dental Care, School of Clinical Dentistry, University of Sheffield, Claremont Crescent, S10 2TA, Sheffield, UK

Received 3 November 2008 ,Revised 5 July 2009 ,Accepted 10 July 2009.

References 

  1. Murdoch-Kinch CA, McLean ME. Minimally invasive dentistry. Journal of American Dental Association. 2003;134:87–95
  2. Toreskog S. The minimally invasive and aesthetic bonded porcelain technique. International Dental Journal. 2002;52:353–363
  3. Qualtrough AJ. Dentine-bonded ceramic crowns: two case reports. British Dental Journal. 1997;183:408–411
  4. Horsted-Bindslev P. Amalgam toxicity: environmental and occupational hazards. Journal of Dentistry. 2004;32:359–365
  5. Rosenstiel SF, Land MF, Fujimoto J. Contemporary fixed prosthodontics. 4th ed.. St. Louis, MO: Mosby Elsevier; 2006;
  6. Crothers A, Wassell RW, Allen R. The resin-bonded porcelain crown: a rationale for use on anterior teeth. Dental Update. 1993;20:388–395
  7. Crocker WP. The cementation of porcelain jacket crowns with adhesive resins. British Dental Journal. 1992;172:64–67
  8. Rammelsberg P, Spiegl K, Eickemeyer G, Schmitter M. Clinical performance of metal-free polymer crowns after 3 years in service. Journal of Dentistry. 2005;33:517–523
  9. Ohlmann B, Dreyhaupt J, Schmitter M, Gabbert O, Hassel A, Rammelsberg P. Clinical performance of posterior metal-free polymer crowns with and without fiber reinforcement: one-year results of a randomised clinical trial. Journal of Dentistry. 2006;34:757–762
  10. Toreskog S, Claes, M. A minimally invasive and esthetic bonded porcelain technique—the concept and the vision. Nordic Dentistry 2003 Yearbook: Quintessence Publishing Group; 2003.
  11. Freedman G. Ultraconservative dentistry. Dental Clinics of North America. 1998;42:683–693ix
  12. Rawlinson A, Winstanley RB. The management of severe dental erosion using posterior occlusal porcelain veneers and an anterior overdenture. Restorative Dentistry. 1988;4:4–6
  13. Burke FJ. Fracture resistance of teeth restored with dentin-bonded crowns: the effect of increased tooth preparation. Quintessence International. 1996;27:115–121
  14. Burke FJ. Maximising the fracture resistance of dentine-bonded all-ceramic crowns. Journal of Dentistry. 1999;27:169–173
  15. Burke FJ, Watts DC. Fracture resistance of teeth restored with dentin-bonded crowns. Quintessence International. 1994;25:335–340
  16. Ohlmann B, Gruber R, Eickemeyer G, Rammelsberg P. Optimizing preparation design for metal-free composite resin crowns. Journal of Prosthetic Dentistry. 2008;100:211–219
  17. Rammelsberg P, Eickemeyer G, Erdelt K, Pospiech P. Fracture resistance of posterior metal-free polymer crowns. Journal of Prosthetic Dentistry. 2000;84:303–308
  18. Calamia JR. High-strength porcelain bonded restorations: anterior and posterior. Quintessence International. 1989;20:717–726
  19. Derand T. Stress analysis of cemented or resin-bonded loaded porcelain inlays. Dental Materials. 1991;7:21–24
  20. Chen JH, Matsumura H, Atsuta M. Effect of different etching periods on the bond strength of a composite resin to a machinable porcelain. Journal of Dentistry. 1998;26:53–58
  21. Burke FJ. Four year performance of dentine-bonded all-ceramic crowns. British Dental Journal. 2007;202:269–273
  22. Burke FJ, Hussey DL, McCaughey AD. Evaluation of the 1-year clinical performance of dentin-bonded ceramic crowns and four case reports. Quintessence International. 2001;32:593–601
  23. Burke FJ, Qualtrough AJ. Follow-up evaluation of a series of dentin-bonded ceramic restorations. Journal of Esthetic Dentistry. 2000;12:16–22
  24. Tsitrou EA, Northeast SE, van Noort R. Evaluation of the marginal fit of three margin designs of resin composite crowns using CAD/CAM. Journal of Dentistry. 2007;35:68–73
  25. Tsitrou EA, Northeast SE, van Noort R. Brittleness index of machinable dental materials and its relation to the marginal chipping factor. Journal of Dentistry. 2007;35:897–902
  26. Tsitrou E, van Noort R. Minimal preparation designs for single posterior indirect prostheses with the use of the CEREC system. International Journal of Computerized Dentistry. 2008;11:227–240
  27. Rusin RP. Properties and applications of a new composite block for CAD/CAM. The Compendium of Continuing Education in Dentistry. 2001;22(Suppl.):35–41
  28. Jung YG, Peterson IM, Kim DK, Lawn BR. Lifetime-limiting strength degradation from contact fatigue in dental ceramics. Journal of Dental Research. 2000;79:722–731
  29. Craig RG. In:  Craig RC editors. Restorative dental materials. St. Louis: Mosby; 1997;
  30. Peterson IM, Wuttiphan S, Lawn BR, Chyung K. Role of microstructure on contact damage and strength degradation of micaceous glass–ceramics. Dental Materials. 1998;14:80–89
  31. Pallis K, Griggs JA, Woody RD, Guillen GE, Miller AW. Fracture resistance of three all-ceramic restorative systems for posterior applications. Journal of Prosthetic Dentistry. 2004;91:561–569
  32. Attia A, Kern M. Fracture strength of all-ceramic crowns luted using two bonding methods. Journal of Prosthetic Dentistry. 2004;91:247–252
  33. Yoshinari M, Derand T. Fracture strength of all-ceramic crowns. International Journal of Prosthodontics. 1994;7:329–338
  34. Ashby MF, Jones DRH. Engineering Materials 2. An introduction to microstructures, processing and design. Elsevier Science Ltd.; 1994;
  35. Attia A, Abdelaziz KM, Freitag S, Kern M. Fracture load of composite resin and feldspathic all-ceramic CAD/CAM crowns. Journal of Prosthetic Dentistry. 2006;95:117–123
  36. Bindl A, Luthy H, Mormann WH. Strength and fracture pattern of monolithic CAD/CAM-generated posterior crowns. Dental Materials. 2006;22:29–36
  37. Strub JR, Beschnidt SM. Fracture strength of 5 different all-ceramic crown systems. International Journal of Prosthodontics. 1998;11:602–609

PII: S0300-5712(09)00178-X

doi: 10.1016/j.jdent.2009.07.003

Journal of Dentistry
Volume 38, Issue 1 , Pages 16-22 , January 2010