Journal of Dentistry
Volume 37, Issue 7 , Pages 549-553 , July 2009

The effect of thermal cycling on metal–ceramic bond strength

Received 14 January 2009 ,Revised 9 March 2009 ,Accepted 21 March 2009.

References 

  1. Giordano RA. Dental ceramic restorative systems. Compendium of Continuing Education in Dentistry. 1996;17:779–782, 784–786 (passim; quiz 794)
  2. Wataha JC. Alloys for prosthodontic restorations. Journal of Prosthetetic Dentistry. 2002;87:351–363
  3. Potiket N, Chiche G, Finger IM. In vitro fracture strength of teeth restored with different all-ceramic crown systems. Journal of Prosthetic Dentistry. 2004;92:491–495
  4. Reitmeier B, Hansel K, Kastner C, Walter MH. Metal–ceramic failure in noble metal crowns: 7-years results of a prospective clinical trial in private practices. International Journal of Prosthodontics. 2006;19:397–399
  5. Walton TR. A 10-year longitudinal study of fixed prosthodontics: clinical characteristics and outcome of single-unit metal–ceramic crowns. International Journal of Prosthodontics. 1999;12:519–526
  6. Walton TR. An up to 15-year longitudinal study of 515 metal–ceramic FPD's: Part 1. International Journal of Prosthodontics. 2002;15:439–445
  7. Pjetursson BE, Sailer I, Zwahlen M, Hämmerle CHF. A systematic review of the survival and complication rates of all-ceramic and metal–ceramic reconstructions after an observation period of at least 3 years. Part I: single crowns. Clinical Oral Implants Research. 2007;18:73–85
  8. Sailer I, Pjetursson BE, Zwahlen M, Hämmerle CH. A systematic review of the survival and complication rates of all-ceramic and metal–ceramic reconstructions after an observation period of at least 3 years. Part II: fixed dental prostheses. Clinical Oral Implants Research. 2007;18:86–96
  9. Bagby M, Marshall SJ, Marshall GW. Metal ceramic compatibility: a review of the literature. Journal of Prosthetic Dentistry. 1990;63:21–25
  10. Lenz J, Schwarz S, Schwickerath H, Sperener F, Schäfer A. Bond strength of metal–ceramic systems in three-point flexure bond test. Journal of Applied Biomaterials. 1995;6:55–64
  11. Shell JS, Nielsen JP. Study of the bond between gold alloys and porcelain. Journal of Dental Research. 1962;41:1424–1437
  12. Hammad IA, Goodkind RJ, Gerberich WW. A shear test for the bond strength of ceramometals. Journal of Prosthetic Dentistry. 1987;58:431–437
  13. Lavine MH, Custer RF. Variables affecting the strength of bond between porcelain and gold. Journal of Dental Research. 1966;45:32–36
  14. Caputo AA, Dunn B, Reisbick MH. A flexure method for evaluation of metal–ceramic bond strengths. Journal of Dental Research. 1977;56:1501–1506
  15. In:  O’Brien WJ,  Craig RG editor. Dental porcelains. Dental material review. Ann Arbor: University of Michigan Press; 1977;p. 123–135
  16. Suansuwan N, Swain MV. New approach for evaluating metal–porcelain interfacial bonding. International Journal of Prosthodontics. 1999;12:547–552
  17. Carter JM, Al-Mudafar J, Soerensen SE. Adherence of a nickel-chromium alloy and porcelain. Journal of Prosthetic Dentistry. 1979;41:167–172
  18. Hammad IA, Talic YF. Designs of bond strength tests for metal–ceramic complexes: review of the literature. Journal of Prosthetic Dentistry. 1996;75:602–608
  19. Lenz J, Kessel S. Thermal stresses in metal–ceramic specimens for the ISO crack initiation test (three-point flexure bond test). Dental Materials. 1998;14:277–280
  20. Fischer J. Ceramic bonding to a dental gold–titanium alloy. Biomaterials. 2002;23:1303–1311
  21. ISO 9693 . Metal–ceramic dental restorative systems. Geneva: International Organization for Standardization; 1999;
  22. Vásquez V, Ozcan M, Nishioka R, Souza R, Mesquita A, Pavanelli C. Mechanical and thermal cycling effects on the flexural strength of glass ceramics fused to titanium. Dental Materials Journal. 2008;27:7–15
  23. Oyafuso DK, Ozcan M, Bottino MA, Itinoche MK. Influence of thermal and mechanical cycling on the flexural strength of ceramics with titanium or gold alloy frameworks. Dental Materials. 2008;24:351–356
  24. Pröbster L, Maiwald U, Weber H. Three-point bending strength of ceramics fused to cast titanium. European Journal of Oral Sciences. 1996;104:313–319
  25. Leibrock H, Degenhart M, Behr M, Rosentritt M, Handel G. In vitro study on the effect of thermo- and load-cycling on the bond strength of porcelain repair systems. Journal of Oral Rehabilitation. 1999;26:130–137
  26. Shimoe S, Tanoue N, Yanagida H, Atsuta M, Koizumi H, Matsumura H. Comparative strength of metal–ceramic and metal–composite bonds after extended thermocycling. Journal of Oral Rehabilitation. 2004;31:689–694

PII: S0300-5712(09)00070-0

doi: 10.1016/j.jdent.2009.03.014

Journal of Dentistry
Volume 37, Issue 7 , Pages 549-553 , July 2009