Journal of Dentistry
Volume 36, Issue 8 , Pages 611-617 , August 2008

Four-year water degradation of a total-etch and two self-etching adhesives bonded to dentin

  • Ali I. Abdalla

      Affiliations

    • Department of Restorative Dentistry, Faculty of Dentistry, University of Tanta, Tanta, Egypt
    • Corresponding Author InformationCorresponding author. Tel.: +20 40 3336654; fax: +20 40 331800.
  • ,
  • Albert J. Feilzer

      Affiliations

    • Department of Dental Materials Science (ACTA), Universiteit van Amsterdam and Vrije Universiteit, Amsterdam, The Netherlands

Received 18 November 2007 ,Revised 18 April 2008 ,Accepted 21 April 2008.

References 

  1. Inoue S, Vargas MA, Abe Y, Yoshida Y, Lambrechts P, Vanherle G, et al. Micro-tensile bond strength of eleven modern adhesives to dentin. Journal of Adhesive Dentistry. 2001;3:237–246
  2. Brackett WW, Dib A, Brackett MG, Reyes AA, Estrada BE. Two year clinical performance of class V resin-modified glass-ionomer and resin composite restorations. Operative Dentistry. 2003;28:477–481
  3. Van Dijken JW. Clinical evaluation of three adhesive systems in class V non-carious lesions. Dental Materials. 2000;16:285–291
  4. Shono Y, Terashita M, Shimada J, Kozono Y, Carvalho RM, Russell CM, et al. Durability of resin–dentin bonds. Journal of Adhesive Dentistry. 1999;1:211–218
  5. Fukushima T, Inoue Y, Miyazaki K, Itoh T. Effect of primers containing N-methylolacrylamide or N-methylolmethacrylamide on dentin bond durability of a resin composite after 5 years. Journal of Dentistry. 2001;29:227–234
  6. De Munck J, Van Meerbeek B, Yoshida Y, Inoue S, Suzuki K, Lambrechts P. Four-year water degradation of a glass-ionomer adhesive bonded to dentin. European Journal of Oral Science. 2004;112:73–83
  7. De Munck J, Van Meerbeek B, Yoshida Y, Inoue S, Vargas M, Suzuki K, et al. Four-year water degradation of total-etch adhesives bonded to dentin. Journal of Dental Research. 2003;82:136–140
  8. Kato G, Nakabayashi N. The durability of adhesion to phosphoric acid etched, wet dentin substrates. Dental Materials. 1998;14:347–352
  9. Sano H, Shono T, Sonoda H, Takatsu T, Ciucchi B, Carvalho R, et al. Relationship between surface area for adhesion and tensile bond strength-evaluation of a micro-tensile bond test. Dental Materials. 1994;10:236–240
  10. Kitasako Y, Burrow MF, Nikaido T, Tagami J. The influence of storage solution on dentin bond durability of resin cement. Dental Materials. 2000;16:1–6
  11. Armstrong SR, Keller JC, Boyer DB. The influence of water storage and C-factor on the dentin–resin composite microtensile bond strength and debonded pathway utilizing a filled and unfilled adhesive resin. Dental Materials. 2001;17:268–276
  12. Armstrong SR, Vargas MA, Fang Q, Laffoon JE. Microtensile bond strength of a total-etch 3-step, total-etch 2-step, self-etch 2-step, and a self-etch 1-step dentin bonding system through 15-month water storage. Journal of Adhesive Dentistry. 2003;5:47–56
  13. Meiers JC, Young D. Two-year composite/dentin bond stability. American Journal of Dentistry. 2001;14:141–144
  14. Burrow MF, Satoh M, Tagami J. Dentin bond durability after three years using a dentin bonding agent with and without priming. Dental Materials. 1996;12:302–307
  15. Giannini M, Seixas CAM, Reis AF, Pimenta LAF. Six-month storage-time evaluation of one-bottle adhesive systems to dentin. Journal of Esthetic Restorative Dentistry. 2003;15:43–49
  16. Ferracane JL, Berge HX, Condon JR. In vitro aging of dental composites in water—effect of degree of conversion, filler volume, and filler/matrix coupling. Journal of Biomedical and Materials Research. 1998;42:465–547
  17. Santerre JP, Shajii L, Leung BW. Relation of dental composite formulations to their degradation and the release of hydrolyzed polymeric-resin-derived products. Critical Reviews in Oral Biology and Medicine. 2001;12:136–151
  18. Feilzer AJ, de Gee AJ, Davidson CL. Setting stress in composite resin in relation to configuration of the restoration. Journal of Dental Research. 1987;66:1636–1639
  19. Hashimoto M, Ohno H, Kaga M, Endo K, Sano H, Oguchi H. In vivo degradation of resin-dentin bonds in humans over 1 to 3 years. Journal of Dental Research. 2000;79:1385–1391
  20. El Zohairy AA, de Gee AJ, de Jager N, van Ruijven LJ, Feilzer AJ. The influence of specimen attachment and dimension on microtensile strength. Journal of Dental Research. 2004;83:420–424
  21. Frankenberger R, Tay FR. Self-etch vs etch-and-rinse adhesives: effect of thermo-mechanical fatigue loading on marginal quality of bonded resin composite restorations. Dental Materials. 2005;21:397–812
  22. Hashimoto M, Ohno H, Kaga M, Endo K, Sano H, Oguchi H. In vivo degradation of resin-dentin bonds in humans over 1–3 years. Journal of Dental Research. 2000;79:1385–1391
  23. Hannig M, Reinhardt KJ, Bott B. Self-etching primer vs phosphoric acid: an alternative concept for composite-to-enamel bonding. Operative Dentistry. 1999;24:172–180
  24. Van Meerbeek B, Dhem A, Goret-Nicaise M, Braem M, Lambrechts P, Vanherle G. Comparative SEM and TEM examination of the ultra structure of resin–dentin interdiffusion zone. Journal of Dental Research. 1993;72:495–501
  25. Kitasako Y, Burrow MF, Nikaido T, Tagami J. The influence of storage solution on bond durability of resin cement. Dental Materials. 2000;16:1–6
  26. Sato M, Miyazaki M. Comparison of depth of dentin etching and resin infiltration with single step adhesive system. Journal of Dentistry. 2005;33:475–484
  27. Tagtekin DA, Yanikoglu FC, Bozkurt FO, Kologlu B, Sur H. Selected characteristics of an Ormocer and a conventional hybrid resin composite. Dental Materials. 2004;20:487–497
  28. Ajlouni R, Bishara SE, Soliman MM, Oonsombat C, Laffoon JF, Warren J. The use of Ormocer as an alternative material for bonding orthodontic brackets. The Angle Orthodontist. 2005;75:106–108
  29. De Munck J, Vargas M, Iracki J, Van Landuyt K, Poitevin A, Lambrechts P, et al. One day bonding effectiveness of new self-etch adhesives to bur-cut enamel and dentin. Operative Dentistry. 2005;30:39–49
  30. Oliveira SS, Pugach MK, Hilton JF, Watanabe LG, Marshall SJ, Marshall GW. The influence of the dentin smear layer on adhesion: a self-etching primer vs. a total-etch system. Dental Materials. 2003;19:758–767
  31. Yoshida Y, Nagakane K, Fukuda R, Nakayama Y, Okazaki M, Shintani H, et al. Comparative study on adhesive performance of functional monomers. Journal of Dental Research. 2004;83:454–458
  32. Misra DN. Adsorption from solutions on synthetic hydroxyapatite: nonaqueous vs. aqueous solvents. Journal of Biomedical and Materials Research. 1999;48:848–855
  33. Carrilho MRO, Carvalho RM, Tay FR, Pashley DH. Effect of storage media on mechanical properties of adhesive systems. American Journal of Dentistry. 2004;17:104–108
  34. Gopferich A. Mechanism of polymer degradation and erosion. Biomaterials. 1996;17:103–117

PII: S0300-5712(08)00134-6

doi: 10.1016/j.jdent.2008.04.011

Journal of Dentistry
Volume 36, Issue 8 , Pages 611-617 , August 2008