Journal of Dentistry
Volume 30, Issue 4 , Pages 161-169 , May 2002

The effect of veneering and heat treatment on the flexural strength of Empress® 2 ceramics

  • M.J. Cattell

      Affiliations

    • Department of Conservative Dentistry, St Bartholomew's and The Royal London School of Medicine and Dentistry, QM, Turner Street, London E1 2AD, UK
    • Corresponding Author InformationCorresponding author. Tel.: +44-207-777000x2160; fax: +44-207-3777375
  • ,
  • R.P. Palumbo

      Affiliations

    • Department of Conservative Dentistry, St Bartholomew's and The Royal London School of Medicine and Dentistry, QM, Turner Street, London E1 2AD, UK
  • ,
  • J.C. Knowles

      Affiliations

    • Department of Biomaterials, Eastman Dental Institute, University College London, 256 Gray's Inn Road, London WC1 8LD, UK
  • ,
  • R.L. Clarke

      Affiliations

    • Department of Conservative Dentistry, St Bartholomew's and The Royal London School of Medicine and Dentistry, QM, Turner Street, London E1 2AD, UK
  • ,
  • D.Y.D. Samarawickrama

      Affiliations

    • Department of Conservative Dentistry, St Bartholomew's and The Royal London School of Medicine and Dentistry, QM, Turner Street, London E1 2AD, UK

Received 30 November 2001 ,Revised 24 July 2002 ,Accepted 26 July 2002.

References 

  1. Pröbster L, Diehl D. Slip-casting ceramics for crown and bridge restorations. Quintessence Int. 1992;21:25–31
  2. Oden A, Anderson M. A new all ceramic crown. Acta Odontol Scand. 1993;51:59–64
  3. McLean JW. A clinical evaluation of recent methods of strengthening dental porcelain. Trans J Br Ceram Soc. 1971;70:124–128
  4. Tinschert J, Zwez D, Marx R, Anusavice KJ. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics. J Dent. 2000;28:529–535
  5. Seghi RR, Sorensen JA. Relative flexural strength of six new ceramic materials. Int J Prosthodont. 1995;8:239–246
  6. Pröbster L. Four year clinical study of glass-infiltrated, sintered alumina crowns. J Oral Rehabil. 1996;23:147–151
  7. Pröbster L. Klinische langzeiterfahrungen mit volkeramischen kronen aus In-Ceram. Quintessenz. 1997;48:1639–1646
  8. Pröbster L. Survival rate of In-Ceram restorations. Int J Prosthodont. 1993;6:259–263
  9. Sorenson JA, Kang SK, Torres TJ, Knode H. In-Ceram fixed partial dentures: Three year clinical trials. J Californian Dent Assoc. 1998;26:207–214
  10. Beham G. IPS Empress; a new ceramic technology. In: Dorsch P, editor. Ivoclar-Vivadent Report, vol. 6; 1990. p. 115.
  11. Wohlwend A, Schaerer P. The Empress technique for the fabrication of full ceramic crowns, inlays and veneers. Quintessenz Zahntech. 1990;16:966–978
  12. Nathanson D. Principles of porcelain use as an inlay/onlay material. In:  Garber DA,  Goldstein RE editor. Porcelain and composite inlays and onlays, aesthetic posterior restorations. Carol Stream, IL: Quintessence Publishing; 1994;p. 32–36
  13. Sorensen JA, Berge HX, Edelhoff D. Effect of storage media and fatigue loading on ceramic strength. J Dent Res. 2000;79:271; Abstract 1017
  14. Sorensen JA, Mito WT, Chamberlain TH. Core ceramic flexural strength from water storage and reduced thickness. J Dent Res. 1999;78:219; Abstract 906
  15. Cattell MJ, Knowles JC, Clarke RL, Lynch E. The biaxial flexural strength of two pressable ceramic systems. J Dent. 1999;27:183–196
  16. Dong JK, Lüthy H, Wohlwend A, Scharer P. Heat-pressed ceramics: technology and strength. Int J Prosthodont. 1992;5:9–16
  17. ASTM, F394-78. Standard test method for biaxial flexure strength (modulus of rupture) of ceramic substrates; 1991. p. 424–8.
  18. Anusavice KJ, Dehoff PH, Fairhurst EW. Comparative evaluation of ceramic–metal bond tests using finite element analysis. J Dent Res. 1980;59:608–613
  19. Abernethey RB. The new Weibull handbook. 2nd ed. Self-published; 1996. p. 7.1–14.
  20. Hölland WH, Schweiger M, Frank M, Rheinberger V. A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass ceramics. J Biomed Mater Res (Appl Biomater). 2000;53:297–303
  21. Kelly JR, Tesk JA, Sorensen JA. Faiure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modelling. J Dent Res. 1995;74:1253–1258
  22. Sorensen JA, Cruz M, Mito WT, Meridith H, Raffeiner O, Foser HP. A clinical investigation on three-unit fixed partial dentures fabricated with a lithium disilicate glass–ceramic. Practical Periodont Aesthet Dent. 1999;11:95–106
  23. Drummond JL, King TL, Bapna MS, Koperski RD. Mechanical property evaluation of pressable restorative ceramics. Dent Mater. 2000;16:226–233
  24. Zeng K, Oden A, Rowcliffe D. Flexure tests on ceramics. Int J Prosthodont. 1996;9:434–439
  25. Chai J, Takahashi Y, Sulaiman F, Chong KH, Lautenschlager EP. Probability of fracture of all-ceramic crowns. Int J Prosthodont. 2000;13:420–424
  26. Correr Sobrinho L, Cattell MJ, Glover RH, Knowles JC. Investigation of the dry and wet fatigue properties of three all ceramic crown systems. Int J Prosthodont. 1998;11:255–262
  27. Faber KT, Evans AG. Crack deflection processes. I. Experiment. Acta Metall. 1983;31:565–576
  28. Thompson JY, Anusavice KJ, Balasubramaniam B, Mecholsky JJ. Effect of microcracking on the fracture toughness and fracture surface fractal dimension of lithia-based glass–ceramics. J Am Ceram Soc. 1995;78:3045–3049
  29. Borom MP, Turkalo AM, Doremus RH. Strength and microstructure in lithium disilicate glass–ceramics. J Am Ceram Soc. 1975;58:385–391
  30. Ansavice KJ, Zhang NZ, Moorhead JE. Influence of colourants on crystallization and mechanical properties of lithia-based glass–ceramics. Dent Mater. 1994;2:141–146
  31. Atkinson DIH, McMillan PW. Glass–ceramics with random and oriented microstructures. Part 3. The preparation and microstructure of an aligned glass–ceramic. J Mater Sci. 1977;12:443–450
  32. McMillan PW. Glass ceramics. 2nd ed.. New York: Academic Press; 1979; p. 150–3
  33. McMillan PW, Phillips SV, Partridge G. The structure and properties of a lithium zinc silicate glass–ceramic. J Mater Sci. 1966;1:269–279
  34. Mormann WH, Bindl A. The cerec 3-A quantum leap for computer-aided restorations: initial results. Quintessence Int. 2000;31:699–712
  35. Hölland WH, Rheinberger S, Frank M. Mechanisms of the nucleation and controlled crystallisation of needle-like apatite in glass ceramics of the SiO2–Al2O3–K2O–CaO–P2O5 system. J Non-Cryst Solids. 1999;253:170–177
  36. Müller R, Abu-Hilal LA, Reinsch S, Hölland WH. Coarsening of needle-shaped apatite crystals in SiO2–Al2O3–Na2O–K2O–CaO–P2O5–F glass. J Mater Sci. 1999;34:65–69

PII: S0300-5712(02)00013-1

Journal of Dentistry
Volume 30, Issue 4 , Pages 161-169 , May 2002